Inconel 718 Nickel Alloy Strip (AMS 5596, UNS N07718)

Inconel 718 Nickel Alloy Strip (AMS 5596, UNS N07718)

Lork Group is a reliable manufacturer and supplier of Inconel 718 strip and coil in China. Alloy 718 is an age-hardenable Nickel-Chromium-Columbium (Niobium)-Molybdenum alloy with high strength, corrosion-resistance, and good fabrication characteristics.
문의 보내기

Inconel 718 strip combines properties that make it suitable for a variety of fabricated component applications in both aircraft turbine engines and land-based turbines. These include seals, bellows, and many types of stamped metal components. The alloy is used in downhole and wellhead components for oil and gas wells.

 

As a leading Inconel strip and coil supplier in China, Lork Group manufactures and produces Inconel 718 strip of various sizes. Contact us as your Alloy 718 Stock Distributor and Supplier.

 

 

0.08 max

0.35 max

0.015 max

0.015 max

0.35 max

17-21

50-55

2.80-3.30

4.75-5.50

0.65-1.15

0.20-0.80

1.00 max

0.006 max

0.30 max

0.05 max

 

 

 


Min (0.2% offset)



(% in 2")

80,000 psi (550 MPa)

140,000 psi (965 MPa)

30 (min)

 

 

Inconel 718 is also used in the oil and gas drilling and production industries due to its high strength and resistance to chlorides, stress corrosion and sulfide stress cracking.

 

 

인기 탭: Inconel 718, Alloy 718, Nickel Strip, AMS 5596, W.-Nr. 2.4668, ASTM B670, precipitation-hardening nickel strip, high-temperature alloy strip